INORGANICCHEMICALSINDUSTRY ›› 2013, Vol. 45 ›› Issue (7): 38-.

Previous Articles     Next Articles

New technology for preparation of stannous octoate by electrochemical method

 WANG  Ya-Xiong-   

  1. Kunming Institue of Precious Metals,Kunming 650106,China
  • Online:2013-07-10 Published:2013-07-16

Abstract: Stannous octoate was prepared by electrochemical method instead of conventional double decomposition method.Effects of electrolyte,agitation speed,current density,voltage,temperature,electrode materials,anti-oxidants,and many other factors on the preparation of stannous octoate were investigated,and the optimum process parameters were obtained.Experi- ment results show that,taking 6 mol/L sodium chloride as electrolyte,metal tin as anode,and titanium plate as cathode,under the conditions of anode current density at 100~120 A/m2,cathode current density at 800~1 000 A/m2,agitation speed of 100 r/min,electrolyte temperature at 60~70 ℃,while adding some antioxidant,stannous octoate product containing 28.32%(mass fraction) Sn2+ and 29.23%(mass fraction) total Sn can be obtained.

Key words: electrochemical method, stannous octoate, metal tin, double decomposition method

CLC Number: