Abstract: <SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">Study of selectively leaching cobalt from copper carbonate ore has been carried out.Reaction and behavior during the copper and cobalt leaching process were analyzed.Effects of the leaching conditions of selectively leaching process were experimentally investigated and the optimum laboratory conditions were confirmed as follows:leaching time was 3 h,leaching temperature was above 70 </SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA">℃</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">,pH was 5,volume ratio of liquid to solid was 5</SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA">∶</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">1,and the amount of CuSO<SUB>4</SUB> at the mass concentration of 27.11 g/L was 1.5 mL.Results showed that the leaching rate of cobalt was 78.37% and the leaching rate of copper was just 0.04% under the above conditions.Effective separation of copper and cobalt was realized and cobalt can be preferentially leached out so as to achieve the full utilization of resources.</SPAN>