Measurement of flame retardant magnesium hydroxide particle size distribution by laser particle size analyzer

Zhou Jing,Han Fengqing,Luo Chongguang,Yan Jianping,Liu Zhiqi   

  • Online:2010-03-10 Published:2010-10-01

Abstract: <SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">A practical,accurate,and rapid method for determination of particle size distribution of flame retardant magnesium hydroxide was established.Factors that influence measurement of particle size of flame retardant magnesium hydroxide powder,such as sample weight,pump speed,dispersing time,dispersing media,dispersant category,and dispersant mass concentration,were investigated by using MS2000 laser particle size analyzer.Suitable conditions for measurement are as follows:with 700 mL water as dispersing medium,with detergent as dispersant,mass concentration of detergent being controlled in 0.1~0.3 g/L,sample weight range of magnesium hydroxide powder in 0.020</SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA">~</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">0.035 g,pump speed in 1 400</SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA">~</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">2 000 r/min,</SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA"></SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">the dispersing time in 2~5 min,and measuring at once after sonication.</SPAN>