Abstract: <SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">Technology of reductive leaching manganese sulfate from low-grade pyrolusite in Hubei province was studied.By using local abundant forestry resources,sawdust can be used as reducing agent in sulphuric acid to leach low-grade pyrolusite.Parameters of the process were studied via orthogonal test and single-factor experiments.Results showed that additive can accelerate the leaching progress of manganese;and the optimum technological conditions of leaching manganese were as follows:leaching temperature was 90 </SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA">℃</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">,mass fraction of sulphuric acid was 25%,leaching time was </SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">1.5 h,</SPAN><SPAN lang=EN-US style="FONT-SIZE: 10.5pt; FONT-FAMILY: "Times New Roman"; mso-bidi-font-size: 12.0pt; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA; mso-fareast-font-family: 宋体">and sawdust and additive consumption accounting for 20% (mass fraction) and 2% (mass fraction) of pyrolusite consumption respectively.Under the optimized conditions,leaching rate of manganese could reach more than 98% and manganese sulfate purity exceeded 98.2%.</SPAN><SPAN style="FONT-SIZE: 10.5pt; FONT-FAMILY: 宋体; mso-bidi-font-size: 12.0pt; mso-ascii-font-family: "Times New Roman"; mso-hansi-font-family: "Times New Roman"; mso-bidi-font-family: "Times New Roman"; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA"></SPAN>