Preparation of lanthanum stannate by precipitation-calcination method

 JIAO  Yun-Hong, YU  Shuang-Hong, SHI   Ling, XU  Jian-Zhong, GUO  Bing-Ru   

  1. College of Chemistry & Environmental Science,Hebei University,Baoding 071002,China
  • Online:2015-05-10 Published:2015-05-06

Abstract: Precursor of lanthanum stannate(La2Sn2O7) was prepared by direct-precipitation method and ammonia sedimenta- tion method respectively,with La(NO)3·6H2O and Na2SnO3·3H2O as main raw materials.The precursor obtained by direct- precipitation method was tested by thermo-gravimetry analysis and was calcinated at different temperatures,then the corre- sponding calcinates were tested by X-ray diffraction(XRD) and the optimum calcination temperature(850 ℃) was confirmed. La2Sn2O7 was obtained by calcinating the precusor at 850 ℃.XRD and scanning electron microscope(SEM) results showed that all target products obtained by the above two methods were cubic crystal structure La2Sn2O7.When the pH=12,the target products obtained by ammonia sedimentation-calcination method and the products prepared by direct-precipitation-calcination method were spherical particles with diameters of about 50 nm,moreover,there were no obvious agglomeration between the particles.

Key words: lanthanum stannate, cubic crystal structure, precipitation-calcination method

CLC Number: